Re: ,.;-~*~-;.,Vistoluk's strat build,.;-~*~-;.,
So i have a bit of a dilema as far as my finishing goes....since i'm sprayign outside.
It's about 100+ degrees here and the humidity is around 85....MN....
I sprayed my first of last 4 coats yesterday (coat 9/12, after I did a complete level sand) when the temp. was down to 90 and humidy to 70 (lateron), but the finish dried really fast and I got alot of blushing. THe lacquer I sprayed was reduced 40%, and i've never had this problem so it must be due to the humidity. any advice on whether what the min. humidity should be before I spray? I just don't want to take any chances, but at the same time, I sort of have a deadline. thanks
|